The plastic deformation behavior and stress-strain response characteristics of Monel alloy at high strain rate ( s≈4.3×10 5s -1 ) are studied using Hopkinson bar and hat-shaped specimen.
采用Hopkinson杆加载技术和帽状试样,研究Monel合金在εs≈4.3×105s-1的高应变速率条件下的应力-应变关系及塑性变形行为。
-
At present, dealing with the apparatus containing oily water has much kind, mainly nature except that oil tank, swash plate except that oil tank, thick grain take except that oil tank, pressure except that oil tank, make up, degrease device, pressure strain pot and single valve strain pot,etc..
目前,处理含油污水的设备有多种,主要包括自然除油罐、斜板除油罐、粗粒化除油罐、压力除油罐、组合除油装置、压力滤罐和单阀滤罐等。
-
According to time-temperature characteristic of hot stamping, tensile experiments were carried out for hot stamping steel USIBOR1500 at the temperature 600℃~800℃ and strain rate 0.01/s~0.5/s on the test machine Gleeble3800 and corresponding stress-strain curves were obtained.
根据热冲压工艺的时间-温度特征,采用Gleeble3800热模拟系统,在温度600℃~900℃、应变速率0.01/s~0.5/s下,对热冲压钢板USIBOR1500进行热拉伸实验,获得了相应的应力-应变曲线。
-
The stress-strain curves of materials at high temperatures and high strain rates can be measured.
在文中给出了一些典型的试验曲线和结果,并对测试方法和结果进行了分析讨论。
-
The boundary condition that the surface of the crust is kept at a constant temperature of 25℃, leads to relatively less obvious variation of temperature in the underground no deeper than 2 kilometers, so that the calculated strain rate is less than 10〓(normal geological strain rate is 10〓~10〓).
由于地表的边界效应,在深度小于2km的地壳里,温度变化相对不急剧,一般不出现大于10〓应变速率(典型的地质应变速率为10〓~10〓)。
-
We obtain the "misfit strain-misfit strain" phase diagram and energy diagram for BST thin film grown on tetragonal base at room temperature.
得到了室温下生长在四方基底上的BST50/50薄膜的&失配应变—失配应变&相图和能量图。
-
We obtain the "misfit strain-misfit strain" phase diagram and energy diagram for BST thin film grown on tetragonal base at room temperature.
用朗道-德文希尔理论研究了非平衡双轴失配应变对单畴外延钛酸锶钡薄膜相变的影响,得到了室温下生长在四方基底上的BST50/50薄膜的&失配应变-失配应变&相图和能量图。
-
The results show that the flow stress increases with the increase of the strain rate, and decreases with the increase of the deforming temperature. The saw tooth fluctuation of the flow stress at higher strain rates and lower temperatures indicates the discontinuous dynamic recrystallization. The flow stress of the aluminum alloy during hot compression deformation can be described by using Zener-Hollomon parameter including Arrhenius item, and the deformation activation energy is 176.54 kJ/mol.
研究结果表明:流变应力随应变速率的增大而增大,随变形温度的升高而降低,在高应变速率和较低温度条件下,应力出现据齿波动,呈不连续再结晶特征;该铝合金热压缩变形的流变应力行为可用包含Arrhenius项的Zener-Hollomon参数来描述,其变形激活能为176.54 kJ/mol。
-
The effects of strain hardening by accumulation of dislocations and the grain structure formed at high strain can be removed by appropriate heat treatment
由于位错的积累和相互阻挡所造成的应变硬化可以通过适当的热处理方法来消除,这种方法称为
-
The strainpath analysis indicates that the deformation of the sheet at the fracture location changes into the plane-strain mode from the stretch mode as the die corner radius is further increased from the optimum value, resulting in an early fracture since the plane-strain mode has a lower forming limit as shown in the FLD of Fig.
当一钢模角落半径是进一步的增加时候调查揭露 formability 是改良的如一钢模角落半径直到最适宜的价值增加,而且变得更更坏地。strainpath 分析指出张的毁坏在破碎位置变化是进入如一钢模角落半径的来自可伸缩的模态飞机-紧张模态之内比较远的从最适宜的价值增加,造成一个早的破碎因为飞机-紧张模态有如图 2 的 FLD 所显示的一个比较低的形成界限。
- 推荐网络例句
-
The split between the two groups can hardly be papered over.
这两个团体间的分歧难以掩饰。
-
This approach not only encourages a greater number of responses, but minimizes the likelihood of stale groupthink.
这种做法不仅鼓励了更多的反应,而且减少跟风的可能性。
-
The new PS20 solar power tower collected sunlight through mirrors known as "heliostats" to produce steam that is converted into electricity by a turbine in Sanlucar la Mayor, Spain, Wednesday.
聚光:照片上是建在西班牙桑路卡拉马尤城的一座新型PS20塔式太阳能电站。被称为&日光反射装置&的镜子将太阳光反射到主塔,然后用聚集的热量产生蒸汽进而通过涡轮机转化为电力